Hardening the wheel.
Jim Young 2 | 24/04/2022 19:29:20 |
48 forum posts 6 photos | A link to the latest in a series. Interesting processes. https://youtu.be/p-8YPOU_GiU
|
Ady1 | 24/04/2022 22:51:25 |
![]() 6137 forum posts 893 photos | This is the interesting bit https://youtu.be/p-8YPOU_GiU?t=1435 I cant believe he did that single handed |
David George 1 | 25/04/2022 06:47:01 |
![]() 2110 forum posts 565 photos | Hi I worked in x factory with a salt bath hardening unit, as an apprentice . We were taught how to use it and made Morse taper drifts and other tools for ourselves including hardening etc. The quenching oil was wale oil we were told and the salt was Sodium cyanide. David Edited By David George 1 on 25/04/2022 06:49:43 |
Trevor Drabble | 25/04/2022 11:17:14 |
![]() 339 forum posts 7 photos | We also used cyanide salt baths to harden sockets , spanners and other associated products when l worked at Gordon Tools in Sheffield. |
Please login to post a reply.
Want the latest issue of Model Engineer or Model Engineers' Workshop? Use our magazine locator links to find your nearest stockist!
Sign up to our newsletter and get a free digital issue.
You can unsubscribe at anytime. View our privacy policy at www.mortons.co.uk/privacy
You can contact us by phone, mail or email about the magazines including becoming a contributor, submitting reader's letters or making queries about articles. You can also get in touch about this website, advertising or other general issues.
Click THIS LINK for full contact details.
For subscription issues please see THIS LINK.