Dan Gelbart is rather dismissive of using solvents to prepare metals for painting. He says a sand blaster, bluing or Ajax, of all things, is best. ...
Suitably chosen solvents are unlikely to damage the surface, whereas abrasives do. Maybe painting implies that scratching and pitting the surface isn't a problem, and it's often done deliberately to provide a key. But abrasives aren't smart if the object is to be anodised.
Degreasing and surface preparation are not the same thing! You abrade the surface so the paint will stick to it mechanically/chemically. You clean the surface of anything that will prevent the paint from sticking to it. This is the last thing you do before opening the paint, and it needs to be done with something that won't leave a residue that's incompatible with the paint. That's why petrol isn't a good cleaner for this purpose. |
Please login to post a reply.
Want the latest issue of Model Engineer or Model Engineers' Workshop? Use our magazine locator links to find your nearest stockist!
Sign up to our newsletter and get a free digital issue.
You can unsubscribe at anytime. View our privacy policy at www.mortons.co.uk/privacy
You can contact us by phone, mail or email about the magazines including becoming a contributor, submitting reader's letters or making queries about articles. You can also get in touch about this website, advertising or other general issues.
Click THIS LINK for full contact details.
For subscription issues please see THIS LINK.