Steve Pavey | 02/01/2016 20:47:24 |
369 forum posts 41 photos | A photo showing the shorter of the two pieces I machined, and the remaining offcut which is probably a bit too far gone. The hammer heads look superb Jack. Is there anything else I can use to etch it with? I have a can of mortar cleaner in the shed, would that work? |
Neil Wyatt | 02/01/2016 22:17:07 |
![]() 19226 forum posts 749 photos 86 articles | Lovely forge-work Jack. |
jaCK Hobson | 02/01/2016 23:38:30 |
383 forum posts 101 photos | Posted by Steve Pavey on 02/01/2016 20:47:24:
. The hammer heads look superb Jack. Is there anything else I can use to etch it with?
Ferric chloride is used to etch circuit boards and you can get it from Maplins. That is the accepted 'best' for etching patterns in metal. You want a weak acid I think. Vinegar will do something. Lemon juice will reveal the pattern but may not etch deeply enough to preserve it for long. Some people claim coffee works. |
Please login to post a reply.
Want the latest issue of Model Engineer or Model Engineers' Workshop? Use our magazine locator links to find your nearest stockist!
Sign up to our newsletter and get a free digital issue.
You can unsubscribe at anytime. View our privacy policy at www.mortons.co.uk/privacy
You can contact us by phone, mail or email about the magazines including becoming a contributor, submitting reader's letters or making queries about articles. You can also get in touch about this website, advertising or other general issues.
Click THIS LINK for full contact details.
For subscription issues please see THIS LINK.