Here is a list of all the postings JohnF has made in our forums. Click on a thread name to jump to the thread.
Thread: Case Hardening |
24/10/2009 15:53:39 |
Hi Peter,
Although you can use the materials suggested i.e. any carbon rich material--chrcoal made from leather, wood, bone etc you need activators added to get good results[bicarbonate of soda is one] As already pointed out coal dust is a no no!
I harden quite a lot of small components and would highly recomend Kasnit or similar to get good consistant results.
I f you want a thick case and are soaking the components for several hours then be aware of grain growth in the core--you need to do a multi heat treatment to relieve this then finally harden the component.
Regards John. |
Thread: Metal filler? |
30/08/2009 10:33:06 |
Depends on the size of hole etc but try Lumiweld allumininum solder --I've use thie to repair al kindes of ally products and it works well.
Alternative ly the suggestion of drilling out to alarger size and fitting a plug [with say loctite] then reworking to your requierments may be best..
John
Edited By Stephen John Fawcett on 30/08/2009 10:33:59 |
Thread: Ground steel bar |
30/08/2009 10:02:27 |
Try J & L Supplies they supply 1m lengths of silver steel, fairly expensive but it will do your job I'm sure http://www.mscjlindustrial.co.uk/cgi/insrhm
Regards John Edited By Stephen John Fawcett on 30/08/2009 10:03:03 |
Want the latest issue of Model Engineer or Model Engineers' Workshop? Use our magazine locator links to find your nearest stockist!
Sign up to our newsletter and get a free digital issue.
You can unsubscribe at anytime. View our privacy policy at www.mortons.co.uk/privacy
You can contact us by phone, mail or email about the magazines including becoming a contributor, submitting reader's letters or making queries about articles. You can also get in touch about this website, advertising or other general issues.
Click THIS LINK for full contact details.
For subscription issues please see THIS LINK.